A processor runs the same PP Resin grade on an injection molding machine and on a single screw extruder in the same week. The injection molded parts show short shots and sink marks, while the extruded profile shows die swell and surface sharkskin. The processor assumes the grade is unsuitable. The real issue is that injection molding and extrusion ask the polymer to do different things. Injection molding asks for low viscosity during filling and fast crystallization during cooling. Extrusion asks for high melt strength during drawing and slow, uniform relaxation at the die. Our factory supplies PP Resin to both processes, and we review the process before recommending a grade. Zhejiang Zhongwang International Trade Co., Ltd. has been supplying polypropylene to converters for over 12 years.

Food-Grade PP Resin



1. Why Does the Same PP Resin Behave Differently in Injection Molding and Extrusion?

In injection molding, the polymer is melted, injected into a closed cavity at high shear rate, packed under pressure, and cooled until it is rigid enough to eject. The cycle is short, and the polymer experiences a rapid temperature drop. In extrusion, the polymer is melted, pumped through a die at a lower shear rate, and drawn into a profile or sheet while it cools in open air or in a water bath. The cycle is continuous, and the polymer experiences a slower cooling rate and a strong extensional flow at the die exit. Our factory sees these differences in the field every month. A grade that flows well in a mold may sag in a die, and a grade that holds melt strength in a die may fill a thin mold section poorly.

The difference is not the chemical identity of the polymer. It is the molecular weight distribution and the melt strength. A narrow molecular weight distribution gives low viscosity at high shear and good filling, which suits injection molding. A broad molecular weight distribution gives high melt strength and resistance to sag, which suits extrusion. Our technical team reviews the part or profile geometry, the cycle time, and the downstream equipment before recommending a grade.


2. How Does Melt Flow Index Decide Which Process a PP Resin Grade Suits?

The melt flow index is the standard measure of how easily the polymer flows under a defined load and temperature. A high melt flow index means low viscosity and easy flow. A low melt flow index means high viscosity and high melt strength. Injection molding usually uses a PP Resin with a melt flow index from 8 to 35 grams per 10 minutes, depending on the wall thickness and the flow length. Extrusion usually uses a melt flow index from 0.3 to 3 grams per 10 minutes, depending on the die swell and the draw down ratio. The table below compares the process requirements.


Process requirement Injection molding Extrusion
Typical melt flow index range 8 to 35 grams per 10 minutes 0.3 to 3 grams per 10 minutes
Dominant flow type High shear filling Low shear pumping and extensional draw
Melt strength requirement Moderate High
Cooling rate Fast, in a metal mold Slow, in air or water
Typical defect if grade is wrong Short shot, sink mark, weld line Die swell, sag, sharkskin, draw resonance

In our factory, we keep separate grades for injection molding and extrusion and we do not recommend substituting one for the other without a trial. A high melt flow grade that fills a thin wall mold will often sag in a profile die because it lacks the melt strength to support its own weight before cooling. A low melt flow grade that holds a profile will often short shot in a thin mold because it cannot flow the required distance before it freezes. Zhejiang Zhongwang International Trade Co., Ltd. provides the melt flow index certificate with each lot and can supply a trial quantity for process evaluation.


3. What Changes in Crystallization and Shrinkage When PP Resin Moves From Mold to Die?

Polypropylene is a semi crystalline polymer, and its final dimensions depend on how much crystallinity develops during cooling. In injection molding, the mold temperature and the cooling time control the crystallinity. A hot mold produces higher crystallinity and higher shrinkage. A cold mold produces lower crystallinity and lower shrinkage, but it can also produce higher molded in stress. In extrusion, the cooling rate is slower and the draw down orients the polymer chains. The orientation increases the strength in the machine direction and increases the shrinkage in that direction when the profile is later heated. Our factory measures the shrinkage of each PP Resin grade in both processes and provides the data to the converter.

The shrinkage difference is why a mold designed for one grade may not produce a dimensionally correct part with another grade. The mold shrinkage for injection molding typically ranges from 1.2 to 2.0 percent, while the extrusion shrinkage after drawing can be 2.0 to 4.0 percent in the machine direction and lower in the transverse direction. The table below shows the typical crystallization and shrinkage behavior.


Behavior Injection molding Extrusion
Crystallinity control Mold temperature and cooling time Cooling bath temperature and draw ratio
Typical mold or die shrinkage 1.2 to 2.0 percent 2.0 to 4.0 percent in machine direction
Orientation effect Low to moderate, near gates High in machine direction
Typical warpage risk Differential cooling and gate location Differential draw and cooling
Annealing effect Relieves molded in stress Relaxes orientation and increases shrinkage

Process engineer's note: The shrinkage data must be measured for the specific process, not taken from a generic data sheet. A PP Resin grade that shows 1.6 percent shrinkage in a mold may show 3.0 percent shrinkage in a drawn profile. In our factory, we measure the shrinkage on a standard test mold and on a standard profile die for each grade, and we provide both values. Zhejiang Zhongwang International Trade Co., Ltd. recommends that the converter run a trial with the actual mold or die before releasing a production order.


4. Why Do Mold Design and Die Design Push PP Resin in Opposite Directions?

Mold design for polypropylene focuses on filling, packing, and cooling. The gate size, the runner layout, and the cooling channel position are selected to avoid short shots and sink marks while keeping the cycle time short. The mold surface is usually polished or textured to control the part appearance. Die design for polypropylene focuses on melt strength, die swell, and draw down. The die land length, the die gap, and the cooling calibration are selected to control the profile dimensions and the surface finish. The two designs are not interchangeable. A mold with a small gate may cause high shear and degradation in extrusion, and a die with a long land may cause excessive pressure in injection molding. Our factory reviews the tool design with the converter before the PP Resin grade is finalized. Zhongwang works with tool makers in the region and can recommend a design review before the steel is cut.

The tool material also matters. Injection molds are often made from hardened steel and are polished to a high gloss. Extrusion dies are often made from stainless steel and are chrome plated to reduce wear and to improve the surface finish. The PP Resin grade must be compatible with the tool material and the surface finish, because a grade with a high filler content can wear the die land and change the profile dimensions over time.


5. How Should Buyers Specify and Verify PP Resin for a Chosen Process?

The purchase order should state the process, the melt flow index range, the density, the tensile yield strength, the notched impact strength, and the shrinkage requirement for that process. The buyer should also state the tool material and the surface finish, because these affect the grade selection. The verification should include the melt flow index certificate, the density certificate, the tensile test report, and the shrinkage test report. Our factory provides all four documents with each lot. We also keep a retained sample for 12 months so that a question about a delivered lot can be checked against the original material. Zhejiang Zhongwang International Trade Co., Ltd. can arrange a trial quantity and a process support visit for a new mold or die.

We recommend that the buyer avoid using a single generic data sheet for both processes. The data sheet may list one melt flow index and one shrinkage value, and the converter may assume that the grade is suitable for both. A short trial on the actual tool will reveal whether the grade flows and shrinks as required. The trial should include a dimensional check after 24 hours, because polypropylene continues to shrink after ejection.


Frequently Asked Questions About PP Resin in Injection Molding and Extrusion

Question 1: Can one polypropylene grade be used for both injection molding and extrusion?

Answer: One grade can sometimes be used for both processes, but the operating window is narrow and the result is usually a compromise. A grade with a medium melt flow index may fill a thick mold section and may also hold a low draw profile, but it may short shot in a thin mold and may sag in a high draw profile. The converter should run a trial on both tools and check the dimensions and the surface finish before releasing the grade for both processes. In most cases, the processor uses two separate grades and keeps them in separate silos to avoid cross contamination.

Question 2: Why does polypropylene shrink more in extrusion than in injection molding?

Answer: Polypropylene shrinks more in extrusion because the draw down orients the polymer chains in the machine direction, and the orientation relaxes when the profile is heated or when it ages. The oriented chains pack more closely in the machine direction, so the shrinkage in that direction is higher than the shrinkage in a molded part. The cooling rate also differs. A molded part cools quickly in a metal mold, which limits the crystal growth, while an extruded profile cools more slowly in air or water, which allows more crystal growth and more shrinkage. The converter should use the shrinkage value measured on the actual process, not a generic value.

Question 3: What documents should a buyer request to verify a polypropylene grade for a specific process?

Answer: The buyer should request the melt flow index certificate, the density certificate, the tensile test report, and the shrinkage test report measured on the relevant process. The buyer should also request the lot number and the date of manufacture, because polypropylene can age and change its flow behavior over time. If the grade contains a filler or an impact modifier, the buyer should request the filler content and the impact strength at the service temperature. A certificate of analysis alone does not show whether the grade is suitable for the process; the shrinkage and flow data are the key documents.

PP Resin performs differently in injection molding and extrusion because the two processes impose different flow, cooling, and orientation histories on the polymer. Injection molding favors a higher melt flow index and fast crystallization in a metal mold. Extrusion favors a lower melt flow index, high melt strength, and controlled draw down. The shrinkage, the tool design, and the verification documents must match the process, not a generic data sheet. When the grade and the process are matched, the converter avoids short shots, sink marks, die swell, and warpage. Our team reviews the process and the tool before recommending a grade and provides the trial support needed to confirm the choice.


Need a process review for a polypropylene injection molding or extrusion project? Contact our technical team to review the part or profile, the tool design, and the required flow and shrinkage data.